Filament › Filament› Basic informationfilament_change_length

Ramming length on extruder change

How many millimeters of filament the nozzle pushes before switching extruder, to ooze less.

How it works

Before switching extruder (printers with two nozzles, like the H2D) or hotend (printers that swap it on their own, like the H2C), the nozzle does a “ramming”: it pushes out a stretch of filament so it doesn't ooze while it waits. On printers with a single extruder and a single hotend, like the A1, these settings do nothing.

When to change it

  • With a single extruder (like the A1): don't touch it; it has no effect.

Typical values

ValueWhat for
5 mmPLA Basicdefault

Watch out for

  • If your printer does switch extruder or hotend and you see strings or leftovers of the previous filament right after the switch, this is the group of settings to look at.

Goes well with

What Bambu Studio saysits help card, quoted

What Bambu Studio says

When changing the extruder, it is recommended to extrude a certain length of filament from the original extruder. This helps minimize nozzle oozing.

Bambu Studio tooltip for this setting · AGPL-3.0

Read more at the official source

In your profileBambu PLA Basic @BBL A1 · 5 mm

In Bambu Studio, the profile Bambu PLA Basic @BBL A1 sets it to5 mm

In other slicers

Orca Slicer
Filament ramming lengthFilament › Basic information
PrusaSlicer
No clear equivalent.
Cura
No clear equivalent.

Names taken from each program's code (Orca Slicer 2.4.2, PrusaSlicer 2.9.6, Cura 5.13.0). Credits